Specification · Kitchen Cabinets
304 vs 201 Stainless Steel: What Is Actually in Your Kitchen Cabinet?
Both alloys look identical, both are called stainless, and both will sit in a dry kitchen for twenty years without a mark. They diverge the moment chloride arrives — and the magnet in your toolbox will not tell you which one you have.
Short answer
304 is an austenitic stainless steel with roughly 18% chromium and 8% nickel. 201 keeps the chromium, roughly halves the nickel to 3.5–5.5%, and substitutes 5.5–7.5% manganese plus nitrogen to recover the strength. Both are legitimate alloys. 201 is not counterfeit steel; it is a cheaper alloy with a narrower job. The fraud is not the metal, it is the paperwork: a 304 quote delivered as 201. The practical test is not a magnet, it is a mill certificate with a heat number traced to the coil, plus an XRF reading taken on the finished part.
Key takeaways
- Both grades are austenitic and both are effectively non-magnetic when annealed, so a magnet proves nothing either way.
- Nickel is the price difference. Halving it from 8% and doubling the manganese is the single largest cost lever in a stainless cabinet, which is exactly why the swap happens.
- The grades diverge under chloride — dishwasher salt, bleach, coastal air — not in a dry upper cabinet.
- Surface condition decides more than grade in many failures: embedded iron from carbon-steel tooling will rust on 316.
- Ask for the heat number on the certificate and match it to the coil, then XRF the finished part. Two checks, thirty seconds, closes the swap.
What the two alloys actually are
Stainless steel is not a coating and it is not a grade of steel with an additive. It is an alloy whose chromium content, above roughly 10.5%, forms a passive oxide layer a few nanometres thick that regenerates itself in air. Everything about the material's behaviour happens in that layer, and the alloy's job is to keep it stable.
304 — UNS S30400, EN 1.4301, the material behind the trade label 18/8 — carries about 18% chromium and 8% nickel. The nickel does something specific and expensive: it stabilises the austenitic crystal structure, which is what makes the alloy ductile, weldable and formable into a deep-drawn sink without cracking.
201 — UNS S20100, EN 1.4372 — keeps the chromium, halves the nickel to 3.5–5.5%, and substitutes manganese at 5.5–7.5% with nitrogen added. Manganese also stabilises austenite, and nitrogen restores the yield strength that the nickel was providing — which is why 201 is, if anything, marginally stronger than 304 rather than weaker. The result is a real austenitic stainless steel that costs materially less, because roughly four points of nickel have been replaced by an element that trades at a fraction of the price.
Which is the whole story in one sentence: the swap exists because nickel is the most expensive element in the alloy by a wide margin, and manganese does a passable imitation of it for a fraction of the cost.
| Grade | Cr | Ni | Other | PREN (approx.) | Magnetic when annealed? | Where it turns up |
|---|---|---|---|---|---|---|
| 304 / 1.4301 / S30400 | 18% | 8% | — | 18–19 | No | The default for food and sanitary equipment. Cabinet boxes, doors, worktops |
| 201 / 1.4372 / S20100 | 16–18% | 3.5–5.5% | 5.5–7.5% Mn, N | 16–21 by formula | No | Cost-down alternative. Common in imported cabinet boxes and internal fittings |
| 430 / 1.4016 / S43000 | 16–18% | nil | Ferritic | ~17 | Yes | Appliance fascias and splashbacks. Will be caught by a magnet |
| 316L / 1.4404 / S31603 | 16–18% | 10–14% | 2–3% Mo | 24–26 | No | Coastal, chlorinated or wash-down environments. Rarely a cabinet default |
PREN — pitting resistance equivalent number, calculated as chromium plus 3.3 times molybdenum plus 16 times nitrogen — is the index normally used to rank grades against chloride. It is arithmetic, so anyone can check it. Applied to this table it produces an uncomfortable result: 316L lands around 25, 304 around 18.5, and a 201 with 17% chromium and 0.25% nitrogen scores about 21 — above 304.
That outcome is the most useful thing on this page. PREN was developed for molybdenum-bearing austenitic grades, and it does not see the two properties that decide how 201 actually behaves in a sink base: the manganese sulphide inclusion population, which is where pitting initiates, and the lower chromium reserve available to repassivate a pit once it has started. The index can rank two alloys as comparable while the metals perform differently, and this is the standard example of it.
An index is a summary, and a summary omits. What it omits here is the entire failure mechanism.

Why the magnet test fails
The magnet test is the most widely repeated piece of advice on this subject and it is wrong twice over.
First, both 304 and 201 are austenitic. Annealed austenite is non-magnetic, so both grades pass a magnet test identically. The test cannot separate them, because there is nothing to separate.
Second, and more confusing in practice, a genuine 304 part is often slightly magnetic. Deep drawing and stamping — exactly the operations used to form a sink or a folded cabinet panel — deform the crystal structure and generate strain-induced martensite, which is ferromagnetic. A formed 304 sink bowl can attract a magnet at the corners. Meanwhile a 201 panel that has been fully annealed will not.
So the test produces false passes and false failures in both directions. What a magnet reliably catches is 430 ferritic steel, which is a different substitution with a different signature: 430 is magnetic in the flat, before any forming. If a cabinet door attracts a magnet across its whole face, you are not looking at 201. You are looking at a ferritic grade.
The version of the test that works. A magnet tells you whether the steel is ferritic. It does not tell you whether it is 304 or 201. For that you need chemistry, and chemistry needs either an XRF gun or a laboratory.
Where the difference becomes visible
In a dry cabinet, 201 and 304 are indistinguishable for the life of the kitchen. Neither will rust, because neither is exposed to anything that breaks the passive layer. The divergence is entirely about chloride.
Chloride attacks the passive film locally, at manganese sulphide inclusions and at grain boundaries, and once a pit starts it is self-propagating: the pit interior becomes acidic and oxygen-starved, and the surrounding metal becomes the anode. This is pitting corrosion, and it is the failure mode that matters here.
Three sources of chloride appear in a normal kitchen, and all three are ordinary rather than exotic:
- Dishwasher salt. Sodium chloride, spilled at the fill port, sitting in the cabinet beside the appliance. This is the single most common cause of pitting inside a stainless kitchen cabinet, and it happens in the least visible place in the room.
- Chlorinated cleaners. Bleach-based sprays and the sodium hypochlorite wipes used by contract cleaners. A wipe-down schedule that is fine on a laminate door is not fine on an unpassivated weld.
- Coastal air. Airborne chloride deposits on every surface in the building. A project 500 m from the sea is a different specification from one 5 km inland, and the difference is not a marketing point.
The reason 201 is worse here is not mysterious. It has less chromium available to rebuild the film, no molybdenum, and a higher manganese sulphide inclusion content, which gives chloride more places to start. None of that appears in the PREN — which is why a supplier who quotes an index number has told you almost nothing about a sink base.
That said: the absolute hours quoted for salt-spray tests are close to meaningless across suppliers, because they depend on surface finish, passivation state, test method and the definition of failure. What survives comparison is the ratio under identical conditions. If you are shown two reports, check that the finish, the method and the failure criterion are identical before reading the numbers.

Which grade belongs where in a kitchen
Treating the whole kitchen as one specification is how projects overpay in some places and fail in others. The room has zones with very different chloride exposure.
| Location | Exposure | 201 acceptable? | What to specify |
|---|---|---|---|
| Upper cabinets and dry storage | Occasional wipe, no standing water | Yes, with no functional penalty | 304 preferred for single-source consistency; 201 defensible if declared |
| Base cabinets away from water | Wipe, occasional spill | Usually yes | 304 if the same finish runs across the room |
| Sink base and the cabinet either side | Standing water, splash, cleaning chemicals | No | 304 minimum. This is where the swap becomes visible |
| Adjacent to the dishwasher | Steam, salt, condensate | No | 304, with sealed edges and a vapour barrier to the appliance |
| Plinth and toe kick | Mopping, pooled water, cleaning agents | No | 304, or a non-metallic plinth. This is the most-wetted surface in the room |
| Coastal or wash-down kitchen | Airborne chloride, hose-down cleaning | No | 316L for exposed faces and welds; 304 elsewhere |
The pattern to notice is that the failure locations are low and wet, while the cost saving is spread across the whole order. Which is why a supplier can swap the grade in the boxes and nobody notices until the sink cabinet blisters in year three — by which time the room is in use and the remedy is a rebuild, not a replacement.
It also explains why the grade question cannot be answered without the carcass question. A 304 sink base that sits in an unsealed particleboard carcase will still fail, just more slowly and for a different reason — which is the subject of which carcass material belongs in a humid kitchen.
The surface matters more than the grade
This is the part that surprises people who have just spent a week arguing about chemistry.
The passive layer is two to three nanometres thick. Its stability depends not only on what the alloy contains but on what the surface has been exposed to. Two mechanisms routinely defeat a perfectly good 304:
Embedded iron. Carbon-steel tooling — a wire brush, a grinding disc, a shear blade, a steel trolley — transfers free iron onto the stainless surface. That iron rusts, and it rusts within days, on 304 and on 316 alike. The stainless underneath is fine; the contamination on top is not. The cure is pickling and passivation to ASTM A380, not a higher grade.
Weld heat tint. Welding burns out chromium at the heat-affected zone and leaves an oxide that is chromium-depleted. That zone is where pitting begins. A ground and polished weld that has not been passivated afterwards is a corrosion initiation site with a decorative finish over it.
So a 201 cabinet that has been properly formed, cleaned and passivated will outlast a 304 cabinet that was brushed with a contaminated wheel. Grade sets the ceiling; surface condition decides whether you get near it.
The finish specification is the same argument one layer up, and it is set out in PVD, powder coat and chrome — where the failure also occurs at a surface nobody specified.

How to verify what you were sold
Four checks, in increasing order of effort and decreasing order of how often they are actually done.
| Method | What it proves | What it cannot prove | Effort |
|---|---|---|---|
| Magnet | Whether the steel is ferritic (430) rather than austenitic | Nothing about 304 versus 201. Both are non-magnetic; formed 304 is often slightly magnetic | Seconds, and unreliable |
| Mill certificate to EN 10204 3.1 | Chemistry of a specific heat, with a heat number | That the metal in your cabinet came from that heat | Minutes, if the paperwork exists |
| Heat number matched to the coil and the delivery | Traceability from certificate to goods. This is the check that closes the swap | Whether the surface has been contaminated since | Half an hour, once per order |
| XRF on the finished part | Actual chemistry of the component in your hand. Detects manganese at 201 levels immediately | Passivation state, weld quality, or the source of the coil | Seconds per reading, with a handheld unit |
The order matters. A mill certificate is a document and documents can be borrowed; a heat number that matches the coil and the delivery note is a chain. An XRF reading on the finished panel is the only check that inspects the object rather than the paperwork, and it is the one that most often finds the problem, because the swap happens at the coil, not at the drawing.
How to write the requirement
- Name the grade and the standard. “304 to EN 1.4301 / UNS S30400”, not “stainless steel” and not “SUS304” alone, which is a Japanese designation that some suppliers use loosely.
- Name the grade by component. Boxes, doors, plinth and worktop are separate line items. A single “stainless” line is where the swap hides.
- Require the certificate and the heat number. EN 10204 3.1, with the heat number stated on the packing list for each delivery.
- State the passivation requirement. Pickled and passivated to ASTM A380 after welding, with the method named.
- State the finish, and the Ra if it will be measured. A 2B mill finish and a brushed 320-grit finish behave differently and are not interchangeable in a specification.
- Reserve the right to XRF. One sentence, and it changes behaviour more than any other clause in the document.
One more clause, for coastal projects: state the distance to the coast on the drawing. It reads as an odd request until a cabinet two streets from the sea fails in year two and everybody discovers the specification was written for an inland site.
How we document it
Bergoto builds stainless steel kitchen cabinets and cabinet components, and the material question is settled in documentation rather than in conversation.
- Grade stated per component on the quotation and the shop drawing, not once for the whole order. (Bergoto detail)
- Mill certificates retained against the delivery, with the heat number carried on the packing list so a site check can be closed without a phone call.
- Welds pickled and passivated as a process step rather than a final wipe, with the method recorded.
- Sample and production from the same alloy source, so the approved sample does not quietly become the better one.
Bergoto is an OEM and ODM manufacturer of bathroom and kitchen products, operating to ISO 9001 quality management and BSCI social compliance, with around thirty years in the industry, ten production lines and annual capacity of roughly 500,000 pieces. Fifteen designers work on product development and project documentation in-house. On a cabinet package, that means the alloy schedule, the drawings and the finish specification come from the team that also runs the line — which is the only arrangement in which a grade claim survives to the third delivery.
If you are comparing quotations that differ by more than the alloy price can explain, send us the two specifications. We will tell you which line item the difference is hiding in, whether or not we win the order.
About these figures
- (standard) — the compositional ranges for 304, 201, 430 and 316L, the EN designations 1.4301, 1.4372, 1.4016 and 1.4404, and the UNS numbers are published alloy specifications. Read the current edition; ranges vary slightly between standards bodies.
- Arithmetic, not estimate. PREN follows from the formula chromium plus 3.3 molybdenum plus 16 nitrogen: give it the same composition and anyone reproduces the same number. Whether that number predicts field behaviour is a separate question, and for manganese-substituted grades it does not — which is the point of the discussion above.
- (standard) — EN 10204 3.1 is the mill certificate type that reports test results for the specific heat; ASTM A380 covers cleaning, descaling and passivation. Both are worth reading rather than citing secondhand.
- (estimate — verify) — relative corrosion performance between grades depends on finish, passivation, test method and failure criterion. Do not carry an absolute hour count from one supplier's report to another; compare only reports produced under identical conditions.
- (Bergoto detail) — per-component grade statements, heat-number traceability and documented passivation describe our standard practice. Confirm against the specification sheet issued for a specific order.
Nothing here replaces a materials engineer's review. Where the environment includes chlorinated water, industrial cleaning agents or a coastal exposure class, the grade decision should be signed off by whoever carries the warranty.
Frequently asked questions
Is 201 stainless steel bad?
No. It is a legitimate austenitic alloy that performs well in dry interior use, which covers most of a kitchen. What is not acceptable is quoting 304 and delivering 201, because the buyer paid for corrosion resistance they did not receive. Judge 201 on where it is used: fine in an upper cabinet, wrong in a sink base or beside a dishwasher.
Does a magnet stick to 304 stainless steel?
Usually not, but often slightly, and that is normal. Annealed 304 is austenitic and non-magnetic; deep drawing and stamping generate strain-induced martensite, which is magnetic, so a formed sink bowl can attract a magnet at the corners. A magnet reliably identifies ferritic grades such as 430, and cannot distinguish 304 from 201 at all.
How can I tell 304 from 201 without a lab?
Match the heat number on the EN 10204 3.1 mill certificate to the coil and the delivery note, then take an XRF reading on the finished part. The XRF separates the two immediately, because 201 carries 5.5–7.5% manganese against roughly 2% in 304, and the reading is unambiguous. Neither the magnet nor a visual inspection will do it.
Is 316 better than 304 for a kitchen?
Only where chloride is continuous: coastal sites, wash-down kitchens, chlorinated water systems. For an inland domestic kitchen, 316 costs more and delivers nothing extra, because the failure mechanism it resists is not present. Spend the difference on passivation and edge sealing first.
Why does new stainless steel rust?
Almost always contamination rather than the alloy. Free iron transferred from carbon-steel tooling, grinding dust or a steel trolley rusts on the surface within days, and weld heat tint leaves a chromium-depleted zone that pits. The remedy is pickling and passivation to ASTM A380, not a higher grade.
Comparing stainless cabinet quotations?
Send us the two specifications and the component list. We will mark which line items can carry the grade claimed at the price quoted, and which cannot — before you place the order.